Título: | The optical absorption of gamma irradiated and heat-treated natural quartz |
Título do periódico: | Materials Research São Carlos |
Autor(es): | Nunes, Eduardo Henrique Martins Lameiras, Fernando Soares |
Afiliação: | Centro de Desenvolvimento da Tecnologia Nuclear/CDTN, Belo Horizonte, MG, Brasil Centro de Desenvolvimento da Tecnologia Nuclear/CDTN, Belo Horizonte, MG, Brasil |
Data do documento: | 2005 |
Palavras-chave: | Quartz;color centers;irradiation;heat treatment |
Resumo: | Quartz with aluminum as impurity absorbs energy from ionizing radiation and modifies its color. Colorless quartz becomes smoky or dark smoky (morion quartz) when exposed to gamma rays. By heat-treatment, smoky quartz may become successively greenish, yellowish, or brownish as the irradiation dose increases. Natural, colorless quartz is routinely colored by irradiation with gamma rays and heat-treatment for jewelry production. The color formation in natural quartz through this procedure is explained based on EPR, UV-VIS, and IR studies of irradiated and irradiated and heat-treated samples. Smoky quartz shows absorption bands in the visible region and a strong EPR signal. After heat-treatment it shows absorption bands in the near UV region with extensions into the visible region and a weak EPR signal. The intensity of the absorption bands is proportional to the irradiation dose. These changes of color are explained by the model of Itoh, Stoneham, and Stoneham. [AlSi O4 /h+]0 centers are produced by irradiation, causing the EPR signal and the absorption bands in the visible region. [AlSi O4]- centers are created from [AlSi O4 /h+]0 centers by heat-treatment. They cannot cause an EPR signal and have absorption bands in the near UV region with extensions into the visible region. The highest concentration of [AlSi O4]- centers occurs when the charge compensators have medium mobility. Lithium should give the best condition for color formation. Sodium (low mobility) and hydrogen (high mobility) should make smoky quartz colorless after heat-treatment. |
Acesso: | L |
Aparece nas coleções: | Artigo de periódico |
Arquivos associados a este item:
Arquivo | Descrição | Tamanho | Formato | |
---|---|---|---|---|
Art-02_Fernando_SLameiras.pdf | 460.47 kB | Adobe PDF | Visualizar/Abrir |
Os itens no repositório estão protegidos por copyright, com todos os direitos reservados, salvo quando é indicado o contrário.